ArcelorMittal

Lamps and connectors for internal and external lighting

 

The stainless steel used has :

- good drawability

- good surface finish and structure

- good pitting resistance

 

 

Ferritic grades: K09 - K30 - K39M - K41
Austénitic grades : 17/7C - 18/9E - 18/9DDQ

Condition : bright annealed (2R) or matt temper rolled (2B)

 

Dimensions :
- thicknesses : 0,20 to 0,80mm
- widths : 7 to 400mm


Form : coils